anticorrosive Floor characteristic:
Affordable Forklift . Long term truck rolling makes the ground highly resistant to corrosion, strong acid and alkali, chemical solvents, impact and cracking. Scope of application: electroplating factory Battery Floors, walls and equipment surfaces of plants, chemical plants, electrolytic cells, pharmaceutical plants, acid-base neutralization pools and other places.
Anti corrosion floor classification:
According to the use function of the anti-corrosion floor, it can be divided into heavy anti-corrosion and light anti-corrosion floor application scope:
1. Electroplating factory, battery factory, chemical factory;
2. Chemical storage area or bucket; Large water tank, electrolytic cell, etc;
3. Sewage and wastewater treatment tank, acid-base neutralization tank.
Construction process:
1. Foundation treatment: Mill High level polishing shall be carried out for floating objects and uneven ground, and dust and sundries shall be removed. If the concave area is too deep, intermediate coating materials shall be used quartz After sand repair, leveling and curing, the primer construction can be carried out;
2. Primer coat: roll coating with resin glue and appropriate diluent to increase adhesion and seal the moisture and moisture on the foundation ground to avoid shelling and delamination of the foundation layer and epoxy coating;
3. Construction of glass fiber cloth and intermediate coating: first pave the glass fiber cloth and then brush the anti-corrosion mortar for intermediate coating. Each layer is brushed with a layer of anti-corrosion mortar for intermediate coating until the specified thickness of the glass fiber anti-corrosion floor is reached;
4. Putty layer;
5 Anticorrosive surface coating: apply two coats of anticorrosive finish resin glue or color paint; Note: The resin used shall be determined according to the design. After coating and scraping, it shall be defoaming with toothed roller holes;
6. During the construction of glass fiber anticorrosive floor, pay attention to the proportion of materials, the method of mixing materials and the time of mixing, so as to avoid the chemical reaction of anticorrosive materials when adding additives to produce a large number of bubbles, which increases the construction difficulty. It also takes a large amount of time to use the toothed roller hole to defoaming. Another situation is that the materials are mixed unevenly, and bubbles are generated after painting, The surface effect of the surface layer will be affected after curing;
7. Finish paint construction: evenly apply the prepared finish paint with a trowel or roller, and the whole ground will be bright and clean after completion, with uniform color and no hollowing;
8. Heavy anti-corrosive finish paint: repeat the prepared finish paint several times to achieve heavy anti-corrosion effect;
9. Completion of construction: people can get on after 24 hours, and heavy pressure can be carried out after 72 hours. (25 ° C shall prevail, and the low temperature opening time shall be appropriately extended).
![](https://img1.bmlink.com/big//supply/2013/7/31/9/217928909332458.jpg)
![](https://img1.bmlink.com/big//supply/2013/7/31/9/663446354988705.jpg)
![](https://img1.bmlink.com/big//supply/2013/7/31/9/221599215744808.jpg)
![](https://img1.bmlink.com/big//supply/2013/7/31/9/274799117015116.jpg)
![](https://img1.bmlink.com/big//supply/569283/2012/9/21/15/587333233834865.jpg)
![](https://img1.bmlink.com/big//default/2012/7/23/10/783708191841705.jpg)
![](https://img1.bmlink.com/big//supply/569283/2012/9/16/15/295509569018851.jpg)